4CrMnSiMoV the chemical composition of steel
C | Si | Mn | P | S | Cr | Mo | V |
0.35~0.45 | 0.80~1.10 | 0.80~1.10 | ≤0.030 | ≤0.030 | 1.30~1.50 | 0.40~0.60 | 0.20~0.40 |
4CrMnSiMoV physical properties of steel
Critical point | Ac1 | Ac3 | Ar1 | Ar3 | Ms | Mf | Bs | Bf |
Temperature (approximate) / ℃ | 792 | 855 | 660 | 770 | 330 | 165 | 420 | 350 |
Item | Heating temperature / ℃ | On forging temperature / ℃ | Final forging temperature / ℃ | Cooling |
Steel ingot Steel billet |
1160~1180 1100~1150 |
1100~1150 1050~1100 |
≥850 ≥850 |
Slow cooling (sand pit or cold) Slow cooling (sand pit or cold) |