Stainless steel 0Cr17Ni12Mo2N
Grade: 0Cr17Ni12Mo2N
Standard: GB / T 1220-1992
● Features and application:
Add 0Cr17Ni12Mo2 in Grade N, increase strength, plasticity is not reduced, so that the material thickness decreases. For better corrosion resistance higher strength components.
● Chemical Composition:
Carbon C: ≤ 0.08
Si Si: ≤ 1.00
Manganese Mn: ≤ 2.00
Sulfur S: ≤ 0.030
Phosphorus P: ≤ 0.035
Chromium Cr: 16.00 ~ 18.00
Ni-Ni: 10.00 ~ 14.00
Mo Mo: 2.00 ~ 3.00
N N: 0.10 ~ 0.22
● Mechanical Properties:
Tensile strength σb (MPa): ≥ 550
Conditions yield strength σ0.2 (MPa): ≥ 275
Elongation δ5 (%): ≥ 35
Reduction of area ψ (%): ≥ 50
Hardness: ≤ 217HB; ≤ 95HRB; ≤ 220HV
● Heat treatment and microstructure specifications:
Standard heat treatment: solution 1010 ~ 1150 ℃ fast-cooling.
Microstructure: Organizing for the austenitic type.
- Phone:021-57866678
021-57866679
Fax: 021-57860199
Cont:Mr.Huang 13818168036
Mr.Zhao 13919185505
Email: shzlgt99@163.com
Website:www.shzlgt99.com
Address:Shanghai fengxian, taikang town highway number 118
0Cr17Ni12mo2N
Public Time:2011年05月13日 | Sort:Made of stainless steel | Hits:960